6. Modeling E#

6.1. Characteristics of modeling#

Monocrystalline behavior DD_CFC. Material point. The law used is MonoCrystal DDCFC .mfront

6.2. Tested sizes and results#

The solution obtained with the Mfront behavior and that obtained with the behavior MONOCRISTAL DD_CFC is compared, by testing the maximum of the relative difference of the following components:

Component

Instant (s)

Reference (difference)

Absolute tolerance

EPZZ

Maximum Deviation

0

1.E-4

rho_1*beta**2

Maximum Deviation

0

1.E-4

1.E-4

_images/100000000000034A00000253D5B4841EE4CC8BA7.png

Constrained curves SIZZ as a function of deformations EPZZ for MFRONT and CODE_ASTER for behavior MONOCRISTAL DD_CFC.