4. B modeling#

4.1. Characteristics of modeling#

Pre-work hardening under tension then cycles with imposed deformation, comparison VISCOCHAB and VISC_CIN2_MEMO. 250 steps of time for 10 cycles.

4.2. Tested sizes and results#

Identification

Instant

VISCOCHAB

VISC_CIN2_MEMO

\(\text{\%}\) difference

\({\sigma }_{\mathit{xx}}\)

\(10\)

\(220\)

\(220\)

0

\({\sigma }_{\mathit{xx}}\)

\(11\)

0

0

0

\({\sigma }_{\mathit{xx}}\)

\(113.5\)

\(3.75459E+02\)

\(3.72353E+02\)

\(\mathrm{-}0.8\)

\({\varepsilon }_{\mathit{xx}}\)

\(113.5\)

\(\mathrm{-}1.87638E\mathrm{-}02\)

\(\mathrm{-}1.87638E\mathrm{-}02\)

0

_images/1000000000000250000001B25F84992841F320B6.jpg

4.3. notes#

The difference of \(\text{0.8\%}\) on the constraints at the final moment fades away if we refine the time step: with a time step twice as fine, the difference becomes \(\text{0.4\%}\).