Benchmark solution ===================== Analytical solutions do not exist. However, experimental results are available (hardness measurements). Benchmark results ---------------------- Thermal calculation: Temperature at points T0, T9, T10 at times :math:`t=\mathrm{13s},\mathrm{20s},\mathrm{30s},` Metallurgical calculation: Hardness profiles at :math:`t=\mathrm{240s}` for segments H5, H10, H10, H10, H15, H25, H35, H38, H45, H55, H55, H65, and H75. Bibliographical references --------------------------- 1. A. Bebey-Fourcot, F. Waeckel, Note EDF DER HI-74/98/003/0. Validation of the metallurgical models of Code_Aster via the simulation of two tempers (July 10, 1998).